1.The material flows behind the wall:
Reason: The material speed is slow, or the material atomization is not good, and the spraying is uneven.
Solution: Adjust the equipment, increase the heating temperature of the pipeline, and improve the heating capacity of the equipment.
2.Uneven foam surface:
Reason: The speed of the material is not coordinated, the nozzle is deformed, and the coating is too thick at a time.
Solution: Adjust the equipment, clean up the material residues in the nozzle, and increase the air source pressure.
3.The material is not out of the square and the price is low:
Reasons: The on-site environment is harsh, the ambient temperature is low, the wind speed is large, and the equipment is blackened. Many reasons can cause the phenomenon of low output.
Solution: Increase the temperature of the material, while shielding the window parts to reduce losses, and reduce construction in windy weather.
4.The material is not well bonded:
Cause: The substrate is polluted by dust and the temperature of the base layer is low.
Solution: Purify the substrate to increase the temperature of the base layer.
5.Block the gun:
Reason: The white material has impurities or the black material enters the water and crystallizes, accompanied by a certain phenomenon of partial material.
Solution: Reduce the heating temperature of the equipment, and at the same time check whether the black and white material pipeline is clogged with impurities.